7097: Plate Alloy Available to Purchase
-
Published:2019
Abstract
Alloy 7097 is a quench insensitive Al-Mg-Zn-Cu-Zr alloy engineered for the most advantageous combination of strength, corrosion resistance, and fracture toughness in thick structural applications. This datasheet provides information on key alloy metallurgy of alloy 7097 and processing effects on mechanical properties of alloy 7097-T7651 plate.
7097: Plate Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 443, https://doi.org/10.31399/asm.hb.v02b.a0006740