7005: Extrusion Alloy
-
Published:2019
Abstract
The extrusion alloy 7005 is used as extruded structural members, where welded or brazed assemblies require moderately high strength and high fracture toughness. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of this 7xxx series alloy.
7005: Extrusion Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 414–415, https://doi.org/10.31399/asm.hb.v02b.a0006728