7449: Very High-Strength Plate and Extrusion Alloy
-
Published:2019
Abstract
This datasheet provides information on key alloy metallurgy and processing effects on mechanical and corrosion performance properties of aluminum alloy 7449. A comparison of toughness and stress-corrosion cracking resistance of alloy 7449 with other alloys is also provided.