7449: Very High-Strength Plate and Extrusion Alloy Available to Purchase
-
Published:2019
Page range:
455 - 456
Abstract
This datasheet provides information on key alloy metallurgy and processing effects on mechanical and corrosion performance properties of aluminum alloy 7449. A comparison of toughness and stress-corrosion cracking resistance of alloy 7449 with other alloys is also provided.
You do not currently have access to this chapter.
Citation
7449: Very High-Strength Plate and Extrusion Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 455–456, https://doi.org/10.31399/asm.hb.v02b.a0006746
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Selected Sources of Information: Corrosion Properties of Materials and Corrosion Testing
Fundamentals of Electrochemical Corrosion
7065 High-Strength, Tough, Corrosion-Resistant Plate
Properties and Selection of Aluminum Alloys
2027 Aerospace Plate and Extrusion Alloy
Properties and Selection of Aluminum Alloys
7097 Plate Alloy
Properties and Selection of Aluminum Alloys
7475 Controlled-Toughness Sheet and Plate Alloy
Properties and Selection of Aluminum Alloys
7255 High-Strength, Fatigue-Resistant Plate
Properties and Selection of Aluminum Alloys
7055 High-Strength Plate and Extrusion Alloy
Properties and Selection of Aluminum Alloys
Effects of Metallurgical Variables on Aqueous Corrosion
Corrosion: Fundamentals, Testing, and Protection
Laser Powder Bed Fusion
Additive Manufacturing Processes
Heat Treatment of Malleable and Compacted-Graphite Irons
Heat Treating of Irons and Steels