2198: Fuselage Sheet Available to Purchase
-
Published:2019
Page range:
318
Abstract
Alloy 2198 is an Al-Cu-Li alloy that is used in combination with 2196-T8 stringers for the fuselage skins of the Bombardier C-Series. This datasheet provides information on composition limits of the alloy 2198 and provides a performance comparison of 2198-T8 and 2024-T351 alloys.
You do not currently have access to this chapter.
Citation
2198: Fuselage Sheet, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 318, https://doi.org/10.31399/asm.hb.v02b.a0006610
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
2324 High-Strength Plate
Properties and Selection of Aluminum Alloys
2050 Al-Cu-Li Alloy
Properties and Selection of Aluminum Alloys
6156 Fuselage Sheet
Properties and Selection of Aluminum Alloys
2055 Low-Density High-Strength Extrusion Alloy
Properties and Selection of Aluminum Alloys
2099 High-Strength, Low-Density Plate and Extrusions
Properties and Selection of Aluminum Alloys
Tribological Properties of Copper Alloys
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Metallurgy and Alloy Compositions
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Stress-Corrosion Cracking of Magnesium Alloys
Stress-Corrosion Cracking: Materials Performance and Evaluation (Second Edition)
2 xxx Aluminum Alloy Datasheets
Properties and Selection of Aluminum Alloys