3004, Alclad 3004, and 3104: Al-Mn-Mg Alloy
-
Published:2019
Page range:
338 - 339
Abstract
This datasheet provides information on key alloy metallurgy of alloys 3004 and 3104, and processing effects on physical and mechanical properties of alloy 3004.
You do not currently have access to this chapter.
Citation
3004, Alclad 3004, and 3104: Al-Mn-Mg Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 338–339, https://doi.org/10.31399/asm.hb.v02b.a0006687
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
6042 Extrusion Alloy
Properties and Selection of Aluminum Alloys
3105 Sheet Alloy
Properties and Selection of Aluminum Alloys
5754 Al-3.1Mg Alloy
Properties and Selection of Aluminum Alloys
6351 Extrusion Alloy
Properties and Selection of Aluminum Alloys
Magnetic Properties
Materials at Low Temperatures
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
1060 99.60 Aluminum Minimum
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys