2014, 2014A and Alclad 2014: High-Strength Alloy Available to Purchase
-
Published:2019
Abstract
This datasheet provides information on key alloy metallurgy, fabrication characteristics, mill-product specifications, processing effects on physical properties, and applications of high-strength alloy 2014. It contains tables that list values of tensile property limits for alloy 2014 flat product, rod, wire, bar, extrusions, and forgings.
2014, 2014A and Alclad 2014: High-Strength Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 292–295, https://doi.org/10.31399/asm.hb.v02b.a0006596