6042: Extrusion Alloy Available to Purchase
-
Published:2019
Page range:
385
Abstract
This datasheet provides information on key alloy metallurgy, and processing effects on physical and mechanical properties of the extrusion alloy 6042. It provides a comparison of characteristics of the alloy 6042 with related alloys and tempers.
You do not currently have access to this chapter.
Citation
6042: Extrusion Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 385, https://doi.org/10.31399/asm.hb.v02b.a0006714
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
5754 Al-3.1Mg Alloy
Properties and Selection of Aluminum Alloys
6351 Extrusion Alloy
Properties and Selection of Aluminum Alloys
3105 Sheet Alloy
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
1060 99.60 Aluminum Minimum
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
Magnetic Properties
Materials at Low Temperatures
Cobalt and Cobalt Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials