Properties and Selection of Aluminum Alloys
5254: Higher-Purity Al-Mg-Cr Alloy
-
Published:2019
Abstract
Alloy 5254 is a higher-purity Al-Mg-Cr alloy used in heat exchangers, steam-jacketed kettles, and pumps. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of this 5xxx series alloy.