6033, 6040, and 6041: Free-Machining Alloys
-
Published:2019
Abstract
This datasheet provides information on composition limits, heat treatment, processing effects on physical and mechanical properties, and applications of free-machining aluminum alloys 6033, 6040 and 6041.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
6033, 6040, and 6041: Free-Machining Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 384, https://doi.org/10.31399/asm.hb.v02b.a0006713
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
Heat Treating of Carbon Steels
Heat Treating of Irons and Steels
Low-Carbon Structural Steels
Light Microscopy of Carbon Steels
6262 Machinable High-Strength Alloy
Properties and Selection of Aluminum Alloys
Nickel-Base Castings
Steel Castings Handbook (Sixth Edition)
Failures of Rolling-Element Bearings and Their Prevention
Analysis and Prevention of Component and Equipment Failures
Dual-Phase Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Wear-Resistant Austenitic Manganese Steels
Metals Handbook Desk Edition (2nd Edition)
355.0 and C355.0 Al-Si-Cu High-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
Dual-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications
Complex-Phase Steels
Advanced-High Strength Steels Science, Technology, and Applications