5154 and 5154A: Al-3.5Mg Alloy
-
Published:2019
Abstract
This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and applications of Al-3.5Mg alloys 5154 and 5154A.
You do not currently have access to this chapter.
Citation
5154 and 5154A: Al-3.5Mg Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 360–361, https://doi.org/10.31399/asm.hb.v02b.a0006699
Download citation file:
Data Ecosystem
The ASM Data Ecosystem arms ASM Members and the scientific community with the tools and data required to exponentially expand the boundaries of materials science to meet the needs of Industry 4.0.
Related Book Content
5050 General-Purpose Alloy
Properties and Selection of Aluminum Alloys
535.0, A535.0, and B535.0 Al-Mg High-Strength Casting Alloy
Properties and Selection of Aluminum Alloys
511.0, 512.0 and 513.0 Al-Mg Moderate-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
7003 Extrusion Alloy
Properties and Selection of Aluminum Alloys
7020 High-Strength Aerospace Alloy
Properties and Selection of Aluminum Alloys
6061 and Alclad 6061 General Structural Alloy
Properties and Selection of Aluminum Alloys