This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and applications of commercially pure aluminum grades 1100 and 1100A. It contains table that lists the standard specifications for 1100 aluminum. The reflectivity of 1100 aluminum as a function of aluminum oxide coating thickness and emissivity of 1100 aluminum foil as a function of coating thickness are illustrated.