Skip Nav Destination
ASM Handbook
Properties and Selection of Aluminum AlloysAvailable to Purchase
Edited by
ASM International
Volume
2B
ISBN electronic:
978-1-62708-210-5
Publication date:
2019
Book Chapter
413.0 and A413.0: Al-Si Die Casting Alloys Available to Purchase
-
Published:2019
Page range:
572 - 573
Abstract
This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and application characteristics of Al-Si die casting alloys 413.0 and A413.0.
You do not currently have access to this chapter.
Citation
413.0 and A413.0: Al-Si Die Casting Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 572–573, https://doi.org/10.31399/asm.hb.v02b.a0006579
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
6082 Medium-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
5050 General-Purpose Alloy
Properties and Selection of Aluminum Alloys
5083 Moderate-Strength Weldable Alloy
Properties and Selection of Aluminum Alloys
6463 Bright-Finishing Extrusion Alloy
Properties and Selection of Aluminum Alloys
7003 Extrusion Alloy
Properties and Selection of Aluminum Alloys
7020 High-Strength Aerospace Alloy
Properties and Selection of Aluminum Alloys