The moderate-strength weldable alloy 5086 provides higher strength than alloy 5052 while maintaining good corrosion resistance in a marine environment. This datasheet provides information on key alloy metallurgy, processing effects on physical and tensile properties, product specifications, and fabrication characteristics of this 5xxx series alloy.