Abstract
The Al-Cu-Li alloy 2050 was designed to replace 2xxx alloys at low thicknesses and 7xxx alloys on the thicker end of the range. This datasheet provides information on key alloy metallurgy and processing effects on mechanical properties of this 2xxx series alloy. A figure presents a performance comparison of 2050 and 7050.
You do not currently have access to this chapter.
Citation
2050: Al-Cu-Li Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 309, https://doi.org/10.31399/asm.hb.v02b.a0006603
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
2055 Low-Density High-Strength Extrusion Alloy
Properties and Selection of Aluminum Alloys
2198 Fuselage Sheet
Properties and Selection of Aluminum Alloys
2099 High-Strength, Low-Density Plate and Extrusions
Properties and Selection of Aluminum Alloys
Principles of Alloying
Alloying Understanding the Basics
Vacuum Infusion
Composites
Out-of-Plane Analysis
Composites
Mechanical Properties of Powder Metallurgy Stainless Steels
Powder Metallurgy
Modeling of Porosity Formation during Solidification
Metals Process Simulation
Mechanical Properties
Understanding How Components Fail (Third Edition)
Component Mechanical Properties
Binder and Polymer Assisted Powder Processing