5083: Moderate-Strength Weldable Alloy
-
Published:2019
Abstract
Alloy 5083 is a moderate-strength weldable alloy differentiated from alloy 5086 by the higher nominal magnesium and manganese contents. This datasheet provides information on composition limits, product specifications, fabrication characteristics, processing effects on physical and mechanical properties, and applications of this 5xxx series alloy.
5083: Moderate-Strength Weldable Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 356–357, https://doi.org/10.31399/asm.hb.v02b.a0006697