Skip Nav Destination
Join ASM Today>
ASM Handbook
Properties and Selection of Aluminum Alloys
Edited by
ASM International
Volume
2B
ISBN electronic:
978-1-62708-210-5
Publication date:
2019
Book Chapter
332.0: Al-Si-Cu Permanent-Mold Casting Alloy
-
Published:2019
Search within book:
Abstract
This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and tensile properties, and applications of Al-Si-Cu permanent-mold casting alloy 332.0.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
332.0: Al-Si-Cu Permanent-Mold Casting Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 536–537, https://doi.org/10.31399/asm.hb.v02b.a0006563
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
336.0 Al-Si-Cu Permanent Mold Casting Alloy
Properties and Selection of Aluminum Alloys
354.0 Al-Si-Cu Premium Casting Alloy
Properties and Selection of Aluminum Alloys
383.0, 384.0, and A384.0 Al-Si-Cu High-Strength Die-Casting Alloys
Properties and Selection of Aluminum Alloys
6151 Aluminum Forging Alloy
Properties and Selection of Aluminum Alloys
5182 Sheet Alloy
Properties and Selection of Aluminum Alloys
5086 and Alclad 5086 Moderate-Strength Weldable Alloy
Properties and Selection of Aluminum Alloys
6069 High-Strength Extrusion Alloy
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys