1060: 99.60 Aluminum Minimum Available to Purchase
-
Published:2019
Page range:
280 - 281
Abstract
This datasheet provides information on key alloy metallurgy and processing effects on physical and mechanical properties of alloy 1060.
You do not currently have access to this chapter.
Citation
1060: 99.60 Aluminum Minimum, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 280–281, https://doi.org/10.31399/asm.hb.v02b.a0006591
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Wrought Titanium and Titanium Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Electroplated Coatings
Corrosion: Fundamentals, Testing, and Protection
Ingot Metallurgy and Mill Products
Titanium: A Technical Guide (Second Edition)
Melting and Conversion
Superalloys: A Technical Guide (Second Edition)
Processing of Titanium and Titanium Alloys
Metals Handbook Desk Edition (2nd Edition)
5754 Al-3.1Mg Alloy
Properties and Selection of Aluminum Alloys
6351 Extrusion Alloy
Properties and Selection of Aluminum Alloys
6042 Extrusion Alloy
Properties and Selection of Aluminum Alloys
3105 Sheet Alloy
Properties and Selection of Aluminum Alloys
Shear, Torsion, and Multiaxial Testing
Mechanical Testing and Evaluation