6009 and 6010: Sheet Alloys
-
Published:2019
Page range:
378
Abstract
The sheet alloys 6009 and 6010 fill the need for materials that would be formed in the soft T4 temper and age harden during the automotive paint-bake cycle. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of these 6xxx series alloys.
You do not currently have access to this chapter.
Citation
6009 and 6010: Sheet Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 378, https://doi.org/10.31399/asm.hb.v02b.a0006710
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
5182 Sheet Alloy
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
7003 Extrusion Alloy
Properties and Selection of Aluminum Alloys
7020 High-Strength Aerospace Alloy
Properties and Selection of Aluminum Alloys
6061 and Alclad 6061 General Structural Alloy
Properties and Selection of Aluminum Alloys
6082 Medium-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
5050 General-Purpose Alloy
Properties and Selection of Aluminum Alloys