2624: Damage Tolerant Plate
-
Published:2019
Abstract
Alloy 2624 was developed by Alcoa as a plate product to replace alloy 2024 and 2324 in applications requiring moderate or high strength and the highest levels of damage tolerance. This datasheet provides information on composition limits, processing effects on physical and mechanical properties, and applications of this alloy. Figures provide comparisons of plane stress R-curves of 2624 with 2024-T351 and 2324-T39 and fatigue crack growth resistance of 2624 with 2024-T351 and 2324-T39.
Sign in
ASM members
Member Sign In2624: Damage Tolerant Plate, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 330–331, https://doi.org/10.31399/asm.hb.v02b.a0006617
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.