2040: High-Temperature Strength Alloy
-
Published:2019
Abstract
Alloy 2040 is a forging alloy with a significant improvement in elevated temperature properties over alloys 2014 and 2219. This datasheet provides information on composition limits of 2040 and provides a comparison of design mechanical properties of 2040 and 2014.
You do not currently have access to this chapter.
Citation
2040: High-Temperature Strength Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 308, https://doi.org/10.31399/asm.hb.v02b.a0006602
Download citation file:
New Handbook: Volume 24A
Volume 24A provides a comprehensive review of additive manufacturing design fundamentals and applications.
Related Book Content
7085 Thick plate and forging alloy
Properties and Selection of Aluminum Alloys
7072 Cladding and Fin Stock
Properties and Selection of Aluminum Alloys
7349 Extrusion Alloy
Properties and Selection of Aluminum Alloys
7076 High-Strength Forging Alloy
Properties and Selection of Aluminum Alloys
2297 and 2397 Plate for Fatigue Critical Applications
Properties and Selection of Aluminum Alloys
2524 Tough Moderate-Strength Sheet and Thin Plate
Properties and Selection of Aluminum Alloys
Mechanical Properties and Testing of Titanium Alloys
Titanium Physical Metallurgy, Processing, and Applications
2196 and 2296 Aerospace Extrusion Alloy
Properties and Selection of Aluminum Alloys
Tribological Properties of Copper Alloys
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Metallurgy and Alloy Compositions
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties