7072: Cladding and Fin Stock
-
Published:2019
Abstract
This datasheet provides information on composition limits, ASTM product specifications, processing effects on physical and mechanical properties, and applications of cladding fin stock 7072.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
7072: Cladding and Fin Stock, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 431, https://doi.org/10.31399/asm.hb.v02b.a0006736
Download citation file:
IMAT Registration
September 12–15, 2022
New Orleans, Louisiana
Keep up to date with the latest materials, applications and technologies. Register today for IMAT 2022!
Related Book Content
7076 High-Strength Forging Alloy
Properties and Selection of Aluminum Alloys
2040 High-Temperature Strength Alloy
Properties and Selection of Aluminum Alloys
7349 Extrusion Alloy
Properties and Selection of Aluminum Alloys
2297 and 2397 Plate for Fatigue Critical Applications
Properties and Selection of Aluminum Alloys
2524 Tough Moderate-Strength Sheet and Thin Plate
Properties and Selection of Aluminum Alloys
Mechanical Properties and Testing of Titanium Alloys
Titanium Physical Metallurgy, Processing, and Applications
2196 and 2296 Aerospace Extrusion Alloy
Properties and Selection of Aluminum Alloys
Tribological Properties of Copper Alloys
Tribomaterials Properties and Selection for Friction, Wear, and Erosion Applications
Metallurgy and Alloy Compositions
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
1 xxx Aluminum Alloy Datasheets
Properties and Selection of Aluminum Alloys