6005, 6005A, and 6105: Medium-Strength Extrusion Alloys
-
Published:2019
Abstract
Alloys 6005 and 6105 were developed in the 1960s to be used in place of alloy 6061 in many applications. This datasheet provides information on chemical composition limits, fabrication characteristics, processing effects on physical and mechanical properties, and applications of medium-strength extrusion alloys 6005, 6005A, and 6105.
6005, 6005A, and 6105: Medium-Strength Extrusion Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 376–377, https://doi.org/10.31399/asm.hb.v02b.a0006709