Book Chapter
2618 and 2618A: Al-Cu-Mg-Ni Alloys for High-Temperature Service
-
Published:2019
Page range:
328 - 329
Abstract
This datasheet provides information on composition limits, key metallurgy, fabrication characteristics, processing effects on physical, tensile, and creep-rupture properties, and applications of Al-Cu-Mg-Ni alloys 2618 and 2618A. The influence of prolonged holding at elevated temperature on tensile properties and the influence of temperature on compressive yield strength of alloy 2618-T61 hand-forged billets are illustrated.
You do not currently have access to this chapter.
Citation
2618 and 2618A: Al-Cu-Mg-Ni Alloys for High-Temperature Service, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 328–329, https://doi.org/10.31399/asm.hb.v02b.a0006616
Download citation file:
Related Book Content
6151 Aluminum Forging Alloy
Properties and Selection of Aluminum Alloys
5182 Sheet Alloy
Properties and Selection of Aluminum Alloys
Structure/Property Relationships
Superalloys: A Technical Guide (Second Edition)
332.0 Al-Si-Cu Permanent-Mold Casting Alloy
Properties and Selection of Aluminum Alloys
5086 and Alclad 5086 Moderate-Strength Weldable Alloy
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
6069 High-Strength Extrusion Alloy
Properties and Selection of Aluminum Alloys