The aluminum alloys 383.0, 384.0, and A384.0 are Al-Si-Cu high-strength die-casting alloys suitable for castings with thin walls and large areas. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and fabrication characteristics of these 3xxx series alloys.