2524: Tough Moderate-Strength Sheet and Thin Plate
-
Published:2019
Abstract
This datasheet provides information on composition limits, processing effects on mechanical properties, and applications of alloy 2524. A comparison of strength minimums and typical damage tolerance properties for Alclad 2524-T3 with Alclad 2024-T3 plate is also provided.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
2524: Tough Moderate-Strength Sheet and Thin Plate, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 326–327, https://doi.org/10.31399/asm.hb.v02b.a0006615
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
7072 Cladding and Fin Stock
Properties and Selection of Aluminum Alloys
2040 High-Temperature Strength Alloy
Properties and Selection of Aluminum Alloys
7076 High-Strength Forging Alloy
Properties and Selection of Aluminum Alloys
7349 Extrusion Alloy
Properties and Selection of Aluminum Alloys
2297 and 2397 Plate for Fatigue Critical Applications
Properties and Selection of Aluminum Alloys
Design Criteria
Composites
Mechanical Properties and Testing of Titanium Alloys
Titanium Physical Metallurgy, Processing, and Applications
2196 and 2296 Aerospace Extrusion Alloy
Properties and Selection of Aluminum Alloys
Damage Tolerance Certification of Commercial Aircraft
Fatigue and Fracture
Design and Certification Considerations
Structural Composite Materials