5xxx Aluminum Alloy Datasheets Available to Purchase
-
Published:2019
Page range:
347
Abstract
This article provides an overview of key metallurgy, properties, and applications of the non-heat-treatable 5xxx series of aluminum alloys. It also shows the relationships between some of the more commonly used alloys in the 5xxx series.
Topics
Wrought aluminum alloys
You do not currently have access to this chapter.
Citation
5xxx Aluminum Alloy Datasheets, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 347, https://doi.org/10.31399/asm.hb.v02b.a0006707
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
3 xxx Aluminum Alloy Datasheets
Properties and Selection of Aluminum Alloys
7 xxx Aluminum Alloy Datasheets
Properties and Selection of Aluminum Alloys