711.0 and 712.0: Natural Aging Casting Alloys
-
Published:2019
Abstract
This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and applications of natural aging casting alloys 711.0 and 712.0. The fatigue strength of smooth and notched permanent mold aluminum casting of C712.0-F is illustrated.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
711.0 and 712.0: Natural Aging Casting Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 587–588, https://doi.org/10.31399/asm.hb.v02b.a0006587
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
308.0 Al-Si-Cu General Purpose Casting Alloy
Properties and Selection of Aluminum Alloys
Wrought Stainless Steels
Properties and Selection: Irons, Steels, and High-Performance Alloys
Properties and Performance of Aluminum Castings
Aluminum Alloy Castings Properties, Processes, and Applications
Processing-Induced Fatigue Fracture of a Helicopter Tail Rotor Blade
Handbook of Case Histories in Failure Analysis
Mechanical Properties of Compacted Graphite Iron
Cast Iron Science and Technology
Electroless Nickel Plating
Surface Engineering
Medical Applications of Stainless Steels
Materials for Medical Devices
Aluminum Casting Alloys and Casting Processes
Aluminum Science and Technology
Permanent Mold Casting of Aluminum Alloys
Aluminum Science and Technology