365.0 (Silafont®-36) and A365.0 (Aural®-2/-3)[1]: Low-Iron Premium Die-Casting Alloys Available to Purchase
-
Published:2019
Abstract
Alloy 365.0 and A365.0 are developed near eutectic Al-Si die-casting alloys with additions of manganese to reduce die soldering. This datasheet provides information on key alloy metallurgy, processing effects on tensile properties, and fabrication characteristics of these 3xxx series alloys.
365.0 (Silafont®-36) and A365.0 (Aural®-2/-3): Low-Iron Premium Die-Casting Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 561–563, https://doi.org/10.31399/asm.hb.v02b.a0006573