2519: Armor Plate and Cryogenic Alloy
-
Published:2019
Page range:
325
Abstract
Alloy 2519 is an Al-Cu alloy that was developed as a higher strength weldable alloy for armor plate. This datasheet provides information on key alloy metallurgy of alloy 2519 and processing effects on mechanical properties of 2519-T87 plate.
You do not currently have access to this chapter.
Citation
2519: Armor Plate and Cryogenic Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 325, https://doi.org/10.31399/asm.hb.v02b.a0006614
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
7039 Armor Plate
Properties and Selection of Aluminum Alloys
Intergranular and Exfoliation Corrosion
Corrosion of Aluminum and Aluminum Alloys
Nonequilibrium Reactions Precipitation Hardening
Phase Diagrams Understanding the Basics
Aluminum Foundry Products
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Heat Treatment Practice of Wrought Age-Hardenable Aluminum Alloys
Aluminum Science and Technology
Principles of Alloying
Alloying Understanding the Basics
Vacuum Infusion
Composites
Out-of-Plane Analysis
Composites
Precipitation-Hardening Stainless Steels
Stainless Steels for Design Engineers
Mechanical Properties
Understanding How Components Fail (Third Edition)