Abstract
The aluminum alloy 4043 is recommended as a filler metal when resistance to salt water corrosion is required, especially when welding such aluminum alloys as 5052, 6061, and 6063. This datasheet provides information on key alloy metallurgy, and processing effects on tensile properties of this 4xxx series alloy.
You do not currently have access to this chapter.
Citation
4043: Welding Filler Metal, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 345–346, https://doi.org/10.31399/asm.hb.v02b.a0006691
Download citation file:
Bi-Weekly Supplement to AM&P Print Magazine
AM&P eNews delivers timely industry news, technology updates, fun videos and facts, and much more to materials professionals from around the globe.
Related Book Content
5052 and 5252 Packaging and General-Construction Alloy
Properties and Selection of Aluminum Alloys
Tensile Properties
Additive Manufacturing Design and Applications
Tensile Properties at High and Low Temperatures and at Room Temperature after High-Temperature Exposure
Aluminum Alloy Castings Properties, Processes, and Applications
Mechanical Properties Data for Selected Titanium Aluminides
Mechanics and Mechanisms of Fracture An Introduction
Squeeze Casting
Casting
Castings
Titanium: A Technical Guide (Second Edition)
Mechanical Properties Data for Selected Aluminum Alloys
Mechanics and Mechanisms of Fracture An Introduction
Mechanical Properties Data for Selected Steels
Mechanics and Mechanisms of Fracture An Introduction
400-Series PM Stainless Steels
Powder Metallurgy Stainless Steels Processing, Microstructures, and Properties
Physical Metallurgy of Beryllium
Beryllium Chemistry and Processing