242.0 and A242.0[1]: Casting Alloys with High-Temperature Strength
-
Published:2019
Abstract
Alloys 242.0 and A242.0 are age-hardenable casting alloys with excellent strength at elevated temperatures. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, fabrication characteristics, and application characteristics of these 2xxx series alloys.