362.0 (Mercalloy 362)[1]: Low-Iron Premium Die-Casting Alloy
-
Published:2019
Abstract
Alloy 362.0, low-iron premium die-casting alloy, is made from recycled secondary metal scrap and was developed to have equivalent or better mechanical properties than Silafont-36 and/or Aural-2. This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and applications of this alloy.
362.0 (Mercalloy 362): Low-Iron Premium Die-Casting Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 560, https://doi.org/10.31399/asm.hb.v02b.a0006572