7049 and 7049A: Extrusion and Forging Alloy Available to Purchase
-
Published:2019
Page range:
421 - 422
Abstract
Alloy 7049 is produced occasionally for forgings and extrusions. This datasheet provides information on key alloy metallurgy and processing effects on physical and mechanical properties of this 7xxx series alloy.
You do not currently have access to this chapter.
Citation
7049 and 7049A: Extrusion and Forging Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 421–422, https://doi.org/10.31399/asm.hb.v02b.a0006732
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
Wrought Aluminum Processes and Products
Aluminum Science and Technology
2014, 2014A and Alclad 2014 High-Strength Alloy
Properties and Selection of Aluminum Alloys
Wrought Titanium and Titanium Alloys
Properties and Selection: Nonferrous Alloys and Special-Purpose Materials
Failure of a Helicopter Main Rotor Blade
Handbook of Case Histories in Failure Analysis
Collapse of Extension Ladders by Overloading of Side Rails
ASM Failure Analysis Case Histories: Household Products and Consumer Goods
Exfoliation Corrosion of HE.15 Aluminium Alloy
ASM Failure Analysis Case Histories: Failure Modes and Mechanisms
2324 High-Strength Plate
Properties and Selection of Aluminum Alloys
2055 Low-Density High-Strength Extrusion Alloy
Properties and Selection of Aluminum Alloys
Ductile Overload Fracture of an Extension Ladder Made From 6061-T6 Aluminum Alloy Extrusions
ASM Failure Analysis Case Histories: Processing Errors and Defects
2099 High-Strength, Low-Density Plate and Extrusions
Properties and Selection of Aluminum Alloys