535.0, A535.0, and B535.0: Al-Mg High-Strength Casting Alloy
-
Published:2019
Abstract
This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and applications of Al-Mg high-strength casting alloy 535.0.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
535.0, A535.0, and B535.0: Al-Mg High-Strength Casting Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 583–584, https://doi.org/10.31399/asm.hb.v02b.a0006585
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
5050 General-Purpose Alloy
Properties and Selection of Aluminum Alloys
357.0 and Variations A357.0 to F357.0 Al-Si-Mg High-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
5154 and 5154A Al-3.5Mg Alloy
Properties and Selection of Aluminum Alloys
511.0, 512.0 and 513.0 Al-Mg Moderate-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
356.0 and A356.0 Al-Si-Mg High-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
6082 Medium-Strength Structural Alloy
Properties and Selection of Aluminum Alloys