Abstract
This datasheet provides information on key alloy metallurgy, processing effects on physical and mechanical properties, and application characteristics of Al-Si-Mg general-purpose die-casting alloys 360.0 and A360.0.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
360.0 and A360.0: Al-Si-Mg General-Purpose Die-Casting Alloys, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 558–559, https://doi.org/10.31399/asm.hb.v02b.a0006571
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
2124 Aerospace Plate Alloy
Properties and Selection of Aluminum Alloys