3xxx Aluminum Alloy Datasheets
-
Published:2019
Page range:
332 - 333
Abstract
This article discusses the major characteristics of the 3xxx series aluminum alloys. It contains a table that lists product specifications of these 3xxx alloys.
You do not currently have access to this chapter.
Citation
3xxx Aluminum Alloy Datasheets, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 332–333, https://doi.org/10.31399/asm.hb.v02b.a0006689
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
5 xxx Aluminum Alloy Datasheets
Properties and Selection of Aluminum Alloys
7 xxx Aluminum Alloy Datasheets
Properties and Selection of Aluminum Alloys