Properties and Selection of Aluminum Alloys
Edited by
ASM International
Volume
2B
ISBN electronic:
978-1-62708-210-5
Publication date:
2019
Abstract
This datasheet provides information on key alloy metallurgy, fabrication characteristics, processing effects on physical and mechanical properties, and application characteristics of Al-Si-Mg high-strength premium casting alloy 359.0.
You do not currently have access to this chapter.
Sign in
Don't already have an account? Register
You could not be signed in. Please check your email address / username and password and try again.
ASM members
Member Sign InCitation
359.0: Al-Si-Mg High-Strength Premium Casting Alloy, Properties and Selection of Aluminum Alloys, Vol 2B, ASM Handbook, Edited By Kevin Anderson, John Weritz, J. Gilbert Kaufman, ASM International, 2019, p 556–557, https://doi.org/10.31399/asm.hb.v02b.a0006570
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.
Related Book Content
357.0 and Variations A357.0 to F357.0 Al-Si-Mg High-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
356.0 and A356.0 Al-Si-Mg High-Strength Casting Alloys
Properties and Selection of Aluminum Alloys
5652 Al-2.5Mg Alloy
Properties and Selection of Aluminum Alloys
7050 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
2026 Aluminum Extrusion Alloy
Properties and Selection of Aluminum Alloys
7075 and Alclad 7075 High-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
6082 Medium-Strength Structural Alloy
Properties and Selection of Aluminum Alloys
5050 General-Purpose Alloy
Properties and Selection of Aluminum Alloys
5083 Moderate-Strength Weldable Alloy
Properties and Selection of Aluminum Alloys
6463 Bright-Finishing Extrusion Alloy
Properties and Selection of Aluminum Alloys