This article is a comprehensive collection of graphs that present information on the hardenability bands of various grades of alloy steels. It also includes figures showing correlations of Jominy equivalent cooling rates, plots of end-quench bands of carbon steels, and logarithmic plots of relative hardenability of carbon steels.