Steel Cross Reference to AISI/SAE Designations Available to Purchase
-
Published:2014
Page range:
572 - 576
Abstract
This article is a compilation of tables that present information on cross-referencing of steel designations that are followed in France, Germany, Italy, Japan, Sweden, and Britain to AISI/SAE.
You do not currently have access to this chapter.
Citation
Steel Cross Reference to AISI/SAE Designations, Heat Treating of Irons and Steels, Vol 4D, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 572–576, https://doi.org/10.31399/asm.hb.v04d.a0006000
Download citation file:
Join ASM International
Being a member of the world’s largest association of materials professionals provides the benefits and resources you need to accomplish your personal and professional goals.
Related Book Content
AISI-SAE System of Designations for Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Cross-Reference to Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
Introduction—Purpose of Text, Microstructure and Analysis, Steel Definitions, and Specifications
Steels: Processing, Structure, and Performance (Second Edition)
Steel as a Material
Metallography of Steels Interpretation of Structure and the Effects of Processing
Introduction
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels
History and Primary Steel Processing
Steels: Processing, Structure, and Performance (Second Edition)
Steel Hardness Conversions
Metallurgy for the Non-Metallurgist (Second Edition)
Glossary of Terms: Surface Engineering
Surface Engineering
Decarburization of Steels
Practical Heat Treating (Second Edition)
Macroetchants Based on Copper-Containing Compounds–For Etching of Iron And Steel
Metallography Principles and Practice