Abstract
This article contains a table that presents information on cross-references to standard SAE carbon and low-alloy steel grades to selected chemically similar steels.
Topics
Cast iron,
Steel,
Carbon steel,
High-alloy steel,
Low-alloy steel,
Tool steel,
Gears,
Heat treatment,
Boron,
Copper
You do not currently have access to this chapter.
Citation
Steel Cross Reference, Heat Treating of Irons and Steels, Vol 4D, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 563–571, https://doi.org/10.31399/asm.hb.v04d.a0005999
Download citation file:
Related Book Content
Hardenability Curves
Properties and Selection: Irons, Steels, and High-Performance Alloys
Hardness Conversions
Steels: Processing, Structure, and Performance (Second Edition)
Carbonitriding Gears
Heat Treatment of Gears A Practical Guide for Engineers
Thermal Properties of Carbon and Low-Alloy Steels
Heat Treating of Irons and Steels
Carbon Steels and Alloy Steels Used in Warm and Hot Working
Induction Heating and Heat Treatment
Cracking on the Parting Line of Closed-Die Forgings
Handbook of Case Histories in Failure Analysis
Introduction to Gear Heat Treatment
Heat Treatment of Gears A Practical Guide for Engineers
Classifications and Designations of Carbon and Alloy Steels
Metals Handbook Desk Edition (2nd Edition)
Forging of Carbon and Alloy Steels
Metalworking: Bulk Forming
Compositions of Standard Alloy Steels
Principles of the Heat Treatment of Plain Carbon and Low Alloy Steels