Heat Treating of Boron Steels
-
Published:2014
Abstract
This article provides a detailed discussion on the effect of boron in heat-treated steel and thermomechanically-simulated steel. It describes the boron hardenability mechanism and the effect of composition and heat treatment parameters on boron hardenability. The article examines the hardening behavior of unalloyed boron steel and low-alloyed boron steel in heat treatment experiments by varying the austenitizing temperatures and cooling conditions. It also discusses the applications of boron steels.
Anjana Deva, Bimal Kumar Jha, Heat Treating of Boron Steels, Heat Treating of Irons and Steels, Vol 4D, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014, p 179–187, https://doi.org/10.31399/asm.hb.v04d.a0005963