Tool steels are an important class of steels due to their distinct applications and their specific heat treating issues. This article provides an overview of the classification and production of tool steels, and discusses the procedures and process control requirements for heat treating principal types of tool steels. It reviews the various heat treating processes, namely, normalizing, annealing, stress relieving, austenitizing, quenching, and tempering, and surface treatments and cold treating. The article also provides information on the applicability of these processes to various types of tool steels.