Reference Information
-
Published:2014
Abstract
This article is a collection of two iron-carbon phase diagrams.
Abstract
This article is a compilation of tables that present information on austenitizing temperatures for direct-hardening carbon and alloy steels, case depth of steels for different carburizing times and temperatures, typical heat treatments for case hardening of carbon and carburizing of alloy steels, as well as direct hardening of carbon steels and alloy steels.
Abstract
Steel, heated in contact with air at temperatures in the tempering range, takes on various temper colors due to the formation of a thin oxide film. This article provides detailed information on temper colors...
Sign in
ASM members
Member Sign InReference Information, Heat Treating of Irons and Steels, Vol 4D, ASM Handbook, Edited By Jon L. Dossett, George E. Totten, ASM International, 2014
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.