Explosion of Air Receiver on Excavator
-
Published:2019
Abstract
While an attempt was being made to start the diesel engine of a dragline type excavator, a severe explosion took place, the operator unfortunately being killed. The engine was normally started by compressed air from an air bottle or receiver charged to a pressure of 350 psi by a small auxiliary engine driven compressor fitted on the excavators. On an occasion when this had broken down, the air bottle was replenished by the engineer-in-charge from a cylinder of compressed air. The compressor engine remained unserviced and when the starting bottle again became depleted, the excavator operator re-charged it himself from another cylinder without the knowledge of the engineer. The engine was started satisfactorily, and the bottle charged again to 350 psi in readiness for the start on the following day. It was while an attempt was being made to start the engine on this occasion that the explosion took place. The cylinder used by the operator for re-charging the receiver contained not air but oxygen.
Explosion of Air Receiver on Excavator, ASM Failure Analysis Case Histories: Improper Maintenance, Repair, and Operating Conditions, ASM International, 2019, https://doi.org/10.31399/asm.fach.usage.c9001488
Download citation file:
New Handbook: Volume 11B
Now available in the Digital Library! Volume 11B serves as a reference and guide to help engineers determine the causes of failure in plastic components and make corrective adjustments through design and manufacturing modifications.