Failure of an Oil Engine Connecting Rod Arising from a Deposit of Weld Metal
-
Published:2019
Abstract
One of the connecting rods of a vertical, four-cylinder engine with a cylinder diameter of 5 in. failed by fatigue cracking just below the gudgeon-pin boss. Failure took place in line with the lower edge of a deposit of weld metal. The fracture surface was smooth, conchoidal, and characteristic of that resulting from fatigue. The origin of the major crack was associated with a crescent-shaped area immediately below the weld deposit. This showed brittle fracture characteristics and appeared to be an initial crack that occurred at the time of welding and from which the fatigue crack subsequently developed. The rod was made from a medium carbon or low-alloy steel in the hardened and fully tempered condition. Evidence indicated that, following modification to the oil feed system, the rod that broke was returned to service with fine cracks present immediately below the weld deposit, which served as the starting points of the fatigue cracks. Following this accident, the remaining three rods (which had been modified in a similar manner) were replaced as a precautionary measure.
Failure of an Oil Engine Connecting Rod Arising from a Deposit of Weld Metal, ASM Failure Analysis Case Histories: Improper Maintenance, Repair, and Operating Conditions, ASM International, 2019, https://doi.org/10.31399/asm.fach.usage.c9001434
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!