ASM Failure Analysis Case Histories: Chemical Processing Equipment
Absorbers, Evaporators, and Condensers
-
Published:2019
Abstract
Several tubes in a tube bundle in an evaporator used to concentrate an acid nitrate solution failed by leakage. The feed to the evaporator contained about 6% nitrate, and the discharge about 60% nitrate. The tube bundle was comprised of type 309S (Nb) stainless steel drawn-and-welded tubes expanded and welded into two type 304L stainless steel tube sheets. The tubes failed by crevice corrosion. The failed tubes were defective as-received, and the establishment of concentration cells within the longitudinal cracks in the seam welds led to ultimate corrosive penetration of the wall. There was no evidence of crevice corrosion...
Sign in
ASM members
Member Sign InAbsorbers, Evaporators, and Condensers, ASM Failure Analysis Case Histories: Chemical Processing Equipment, ASM International, 2019
Download citation file:
ASM Technical Books
ASM Technical Books offer a wealth of materials science and engineering knowledge from experts in the field. Discover hundreds of practical guides and reference resources on a wide variety of subjects.