Brittle Rupture of a Chain Sling
-
Published:2019
Abstract
While a chain sling was being used to lift a casting one of the links ruptured. The sling, reputed to be of the electrically-welded steel type, was at least eight years old and had been overhauled several times during its working life. Examination showed the links were scarf-welded. Furthermore, the welds were at the ends and not at the sides as is usual in the case of electrically-welded chains. A transverse section from one side of a link was examined microscopically. This showed the material to be wrought-iron of satisfactory quality. It was concluded this chain sling had been made from wrought-iron, forge welded in the usual manner, and that it was not electrically-welded steel as had been supposed. Failure was attributed to embrittlement in service of the surface material of the links. If it had been realized that the sling was made from wrought-iron then it would doubtless have been subjected to periodical annealing in accordance with Statutory requirements, which would have restored the ductility of the surface material.
Brittle Rupture of a Chain Sling, ASM Failure Analysis Case Histories: Material Handling Equipment, ASM International, 2019, https://doi.org/10.31399/asm.fach.matlhand.c9001453
Download citation file:
October 16-19 | Detroit, Michigan
Keep up to date with the latest materials and processing technologies. Register today for IMAT 2023 & Heat Treat 2023!