Brittle Failure of Reformer Tube During Pressure Test
-
Published:2019
Abstract
During periodic inspection of the tubes of a reformer furnace, a soapy water leak test with the tubes pressurized with nitrogen was being carried out by site personnel in a manner contrary to the policy of the organization when one of the tubes suddenly disintegrated with explosive violence. The tube approximately 30 ft. long by 6 in. diam, was constructed of three spun cast sections butt welded together. The material specified for tubes for this service was basically a 25% chromium, 20% nickel, cast stainless steel containing 0.4% carbon to optimize creep resistance. Failure initiated in the region of...
Sign in
ASM members
Member Sign InBrittle Failure of Reformer Tube During Pressure Test, ASM Failure Analysis Case Histories: Failure Modes and Mechanisms, ASM International, 2019, https://doi.org/10.31399/asm.fach.modes.c9001475
Download citation file:
March 14-16 | Fort Worth, Texas
Keep up to date with the latest aerospace materials and technologies. Register today for Aeromat 2023!