A 2 ft. diam 20 ft. long cylinder with a wall thickness of 1 in. used for the transportation of a compressed gas failed by cracking. The cylinder was forged in a low ally steel. The working pressure was 3000 psi and it had been in service for about seven years. A longitudinal crack, about 2 in. long, developed at the approximate mid-length of the vessel, and allowed slow de-pressurization. Subsequent examination by radiography and ultrasonic means indicated the crack was associated with an irregularly shaped, laminar type of defect located within the wall of the vessel. It was...